Extraction of V2O5 from stone coal containing Vanadium from Westnorth China is investigated. The results show that Vanadium of about 80% can be leached with sulfuric acid under the condations that temperature is 85℃, mass ratio of liquid and solid is 1∶1, ore size is -60 mesh. Then puritic solution containing V2O5 can be acquired after being extracted with P204 and TBP dissolved in sulfonated kerosene and stripped with sulfuric acid. Refine V2O5 (purity is 98%) can acquired by precipitating with ammonium water and pyrolysis.
[1] GodardJB.SaltRoastingofVanadiumOres[C].ExtrMet-allMetProcSymp.1981.127-45.
[2] BrooksPT,PottrGM.RecoveringVanadiumfromDolomiticNerada,MBRI7932,1974.20.
[3] 煤碳部综合利用和科技情报石煤湖南分站,湖南石煤综合利用研究所.曼斯菲尔德碳质页岩的开采与加工[J].石煤科技,1979,(3):5-10
[4] 浙江省煤碳工业局.石煤的综合利用[M].北京:煤碳工业出版社.1980.
[5] 浙江农业大学.应用细菌浸出石煤中钒的研究[J].第1集.1978.9.
[6] 梅里特RC.铀的提取冶金学[M].北京:科学出版社,1978.
[7] Seeton.F.A.SolventExtractionRecoversVecoveryVanadiumfromWasteStream[J].ChemEng,1964,71(44):112-114.
[8] CorloGiavarini.RecoveryofVanadiumfromAsh-leachingsolutionbysolventExtraction[J].Fuel,1982,61(6):549-552.
Basic Information:
DOI:10.13355/j.cnki.sfyj.2002.04.002
China Classification Code:TF841.3
Citation Information:
[1]LU Zhaoling(Beijing Research Institute of Chemical Engineering and Metallurgy,CNNC,Beijing101149,China).Investigation and Industrial Practice on Extraction of V_2O_5 from Stone Coal Containing Vanadium by Acid Process[J].Hydrometallurgy of China,2002(04):175-183.DOI:10.13355/j.cnki.sfyj.2002.04.002.